This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2016, 7, 1421–1427, doi:10.3762/bjnano.7.133
Figure 1: SEM image (a) and Raman spectrum (b) of the GO platelets deposited on SiO2/Si wafer.
Figure 2: SEM images of the obtained samples based on graphene and zinc oxide at low (a) and high (b) magnifi...
Figure 3: (a) EDX spectrum and (b) quantitative analysis of the hybrid structure based on GO and ZnO annealed...
Figure 4: Dynamical response of ZnO and RGO–ZnO structures at 250 °C and RH = 50% @ 20 °C: (a) towards 50 and...
Figure 5: Schematic diagram of the sensing mechanism between acetone and the RGO–ZnO structure: Oxygen is abs...
Figure 6: Response of RGO–ZnO and pristine ZnO nanostructures towards 100 ppm acetone and ethanol at a workin...
Figure 7: Calibration curve for acetone at an operating temperature of 250 °C and in a humid air background (...